ISHLATILGAN TEMIR-XROMLI KATALIZATORNI MEXANOKIMYOVIY MODIFIKATSIYALASHDA FAZA O‘ZGARISHLARI VA XROM SHAKLLARINI NAZORAT QILISH
Keywords:
Kalit so‘zlar: mexanokimyoviy faollashtirish, planetar tegirmon, ishlatilgan katalizator, amorfizatsiya, magnetit, maghemit, Cr(III), Cr(VI).Abstract
Annotatsiya. Ishlatilgan temir-xromli katalizatorni planetar tegirmonda mexanokimyoviy faollashtirishda faza tarkibi, dispersligi va xrom shakllarining o‘zgarishi o‘rganildi. 60 daqiqa maydalashda kristallit o‘lchami 42 dan 14 nm gacha kamayib, solishtirma sirt 62 m²/g ga yetadi. Havoda quruq maydalash Cr(VI) miqdorini 0,57 % gacha oshiradi, etanol muhitida esa u 0,05 % gacha kamayadi. Etanol muhitida 60 daqiqa maydalash optimal sharoit sifatida taklif etiladi.
References
1. Boldyrev V.V. Mechanochemistry and mechanical activation of solids // Russian Chemical Reviews. – 2006. – Vol. 75, No. 3. – P. 177–189.
2. Baláž P. Mechanochemistry in Nanoscience and Minerals Engineering. – Berlin: Springer, 2008. – 413 p.
3. Cornell R.M., Schwertmann U. The Iron Oxides: Structure, Properties, Reactions, Occurrences and Uses. – 2nd ed. – Weinheim: Wiley-VCH, 2003. – 664 p.
4. Назаров С.И., Ортиков Ш.Ш., Назаров Ж.И. Синтез и исследование физико-механических свойств эпоксидно-полисульфидных композиционных материалов // Universum: технические науки. 2025. №10 (139).
5. Назаров С.И., Раззаков Х.К., Назаров Н. И. Синтез и физико-химическое исследование гидрофобного корозионностойкого полисульфидного покрытия на основе полисульфида натрия, эпоксидной смолы ЭД-20 и 1,2,2,3-тетрахлорпропана. Universum: технические науки, 7 (10 (139)), 11-16.